Outline
Designed with a concept in which combustion of the polymer
is inducted by pyrolysis at the first stage, then the pyrolyzates
are burned at the second stage.
Feature
•Combustion gas analysis from polymers can be
easily performed.
•Higher molecular weight of the combustion
components can be detected.
•Combustion components are completely removed
in the combustion cell.
•Polymer can be pryolyzed in the atmospheric
environment.
Specification
♦Combustion method: Pyrolysis, then burn
♦Combustion tube: 14 ID X 120 mm
♦Pyrolysis method: Curie point
♦Ignition coil: N-Cr wire
♦Temp. of combustion cell: Ambient to 200°C
♦PAT temp.: Ambient to 200°C
♦Air or oxygen: 0 to 500 ml/min
♦Dimensions: 280 W X 300 H X 440 D (mm)
♦Power supply/weight:
AC 100 to 115 V, 8 A/27.5 Kg
|

|